Electrolytes for applying precious metal coatings

All electrolytes have high levels of shine and hardness; the achieved deposits are durable, have high concentrations of reactive metal, are made using distilled or de-mineralized water, using only tested CP and high grade chemicals, and in full compliance with the technology and workability of the working solution.

Before precious metal plating, to degrease the surface, we normally use standard degreasing agents.

Electrolyte Metal content per mass, g/L Electrode material Working temperature of the electrolyte, °С Cathodic density of current, А/dm2 Manufacturer Photo Price per liter
SILVER 22 Silver, titanium with iridium or platinum coating 30 0,1-1,0 “IMP Gold” (Russia) 11500 Р В корзину
PALLADIUM 5,2 titanium with iridium or platinum coating 20-35 0,2-1,0 ”AZoM” (Germany) 42400 Р В корзину
GOLD 24carat 2,2 Stainless steel, titanium with iridium or platinum coating 25-35 0,3 – 1,3 “IMP Gold” (Russia) 27500 Р В корзину
“PINK” GOLD 16Carat 2,5 titanium with iridium or platinum coating 20-30 0,2 - 1,2 “IMP Gold” (Russia) 54800 Р В корзину
“GREEN” GOLD 14carat 2,3 titanium with iridium or platinum coating 20-25 0,2 - 1,2 “IMP Gold” (Russia) 27800 Р В корзину
RADIUM* 1 titanium with iridium or platinum coating 25-30 0,1 - 1,0 ”Cohler” (USA) 34500 Р В корзину
“BLACK” RADIUM* 1 titanium with iridium or platinum coating 25-30 0,1 - 1,0 ”Cohler” (USA) 36200 Р В корзину
PLATINUM 4 titanium with iridium or platinum-coated 20-25 0,2-1,0 “IMP Gold” (Russia) 43500 Р В корзину

* — Bright white or greyish-black metallic coating. Radium can be directly applied to silver, gold, nickel and nickel alloys. The main e characteristics of this electrolyte are high dependability, lowly sensitivity to dirt, and the highly reflective properties of the deposited layer. It can be mixed with distilled water to bring it up to the needed volume.